COOLTHERM EP-340

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-340

Main features

  • 1.5 W/(m K) Thermal Interface
  • 7,000 to 60,000 cP Mixed Viscosity
  • Low Cured Coefficient of Linear Thermal Expansion

Product Description

CoolTherm® EP-340 Epoxy Resin is a black, filled epoxy resin formulated for use with Thermoset® Hardener No. 18, No. 67, or No. 70. The selected hardener determines the mixed viscosity, working life, cure schedule, operating-temperature capability, and cured mechanical and electrical properties. The resin has a typical viscosity of 300,000 cP at 25 °C and forms thermally conductive encapsulation systems with a typical cured thermal conductivity of 1.5 W/m·K by ISO 22007-2. Its low coefficient of thermal expansion supports applications where expansion and contraction of the cured epoxy encapsulation must be controlled.

Key features

  • Configurable epoxy system: Compatible with three documented Thermoset hardeners for room-temperature cure, elevated-temperature cure, or lower-viscosity processing.
  • Thermally conductive encapsulation: Each documented cured system provides a typical thermal conductivity of 1.5 W/m·K using the Hot Disc Transient Method, ISO 22007-2.
  • Controlled thermal expansion: Cured-system coefficients of linear thermal expansion range from 28 to 31 ppm/°C, depending on the selected hardener.

Applications / Suitable for

  • Thermally conductive epoxy potting and encapsulation
  • Encapsulation systems requiring controlled expansion and contraction
  • Automated meter/mix/dispense processing in high-volume production

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Black Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
2.4
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
300000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical resin and mixed-system properties before cure. Values for mix ratio, viscosity, working life, and cure schedule depend on the selected Thermoset hardener and are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid — CoolTherm EP-340 resin as supplied
Viscosity 300,000 cP Resin at 25 °C; test method not stated
Specific gravity 2.4 — Resin; test temperature and method not stated
Mix ratio by weight 100:3.5 / 100:6.0 / 100:7.0 Resin:hardener Thermoset Hardener No. 18 / No. 67 / No. 70
Mix ratio by volume 100:8.5 / 100:15.5 / 100:16.5 Resin:hardener Thermoset Hardener No. 18 / No. 67 / No. 70
Mixed viscosity 60,000 / 7,000 / 10,000 cP At 25 °C; Hardener No. 18 / No. 67 / No. 70
Working life 40 / 60–120 / 100 minutes At 25 °C; Hardener No. 18 / No. 67 / No. 70
Shelf life 6 months Stored at 25 °C in the original, unopened container; periodically rotate container to minimize settling

 

Technical properties

After-processing / final-state properties

Typical cured properties for CoolTherm EP-340 systems prepared with Thermoset Hardener No. 18, No. 67, or No. 70. Values are listed in that order and are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 1.5 / 1.5 / 1.5 W/m·K Hot Disc Transient Method, ISO 22007-2
Coefficient of linear thermal expansion 28 / 28 / 31 ppm/°C Temperature region and test method not stated
Hardness 92 / 95 / 90 Shore D Hardener No. 18 / No. 67 / No. 70
Tensile strength at 25 °C 43.42 (6,300) / 50.33 (7,300) / 64.81 (9,400) MPa (psi) Test method not stated
Elongation at break 2.2 / 2.7 / 4.1 % Test method not stated
Moisture absorption 0.10 / 0.08 / 0.17 % 24 hours at 25 °C; exposure medium and method not stated
Volume resistivity at 25 °C 2 × 1016 / 5 × 1016 / 6 × 1015 ohm-cm Test method not stated
Dielectric strength 16.1 (410) / 16.1 (410) / 16.9 (430) kV/mm (V/mil) ASTM D149

 