Circalok™ 6410 A/B Urethane Encapsulant is a two-component polyurethane casting elastomer formulated for tooling, mechanical goods, and model-making applications. The black mixed material has a typical viscosity of 600 cP at 25°C, supporting pouring and automatic meter/mix/dispense application. It uses a 17.5:10 resin-to-hardener ratio by weight and provides a typical 30-minute working life at 25°C. The system initially cures in 4 hours at 25°C or 1 hour at 65°C, with complete cure after one week at 25°C. The cured elastomer is flexible, with 55 Shore 00 hardness, 2.6 MPa tensile strength, and 700% elongation at break.

Key features

  • Low mixed viscosity: 600 cP at 25°C supports pouring and meter/mix/dispense processing.
  • Flexible cured elastomer: 55 Shore 00 hardness and 700% elongation at break.
  • Room-temperature or mild heat cure: initial cure in 4 hours at 25°C or 1 hour at 65°C.
  • Controlled two-part processing: 17.5:10 resin-to-hardener mix ratio by weight.
  • Broad documented operating range: -50°C to +105°C.

Applications

  • Tooling and mould-making applications
  • Mechanical goods and flexible cast parts
  • Model-making and prototype casting

Technical Specifications

General Properties
Color
The color
6410 A Resin: Black Liquid | 6410 B Hardener: Amber Liquid | Mixed: Black Liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
A: 1.02 | B: 1.00 | Mixed: 1.04
Physical Properties
Viscosity (Part A)
1250 mPa.s
Viscosity (Part B)
95 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
700 %

Additional Information

Two-part polyurethane casting elastomer

Circalok™ 6410 A/B Urethane Encapsulant

A low-viscosity, two-component polyurethane system for room-temperature mixing, pouring, and curing in tooling, mechanical-goods, and model-making applications. The mixed material flows readily before curing to a soft, flexible black elastomer. A mild 65°C heat cycle can shorten the initial cure where the assembly and process permit.

Two-component urethane 600 cP mixed viscosity 30-minute working life 55 Shore 00 Room-temperature or 65°C cure
Circalok 6410 A/B Urethane Encapsulant resin and hardener packaging

Circalok 6410 A/B Urethane Encapsulant resin and hardener packaging

As supplied and mixed

Component and mixed-material properties

The resin is a black liquid and the hardener is an amber liquid. After mixing at the specified ratio, the system forms a black liquid with a lower viscosity than the resin component. Values are typical and are not specification limits.

Property 6410 A resin 6410 B hardener Mixed material
Appearance Black liquid Amber liquid Black liquid
Viscosity at 25°C 1,250 cP 95 cP 600 cP
Specific gravity 1.02 1.00 1.04
Working life at 25°C 30 minutes after mixing
Processing

Mix, de-air when needed, pour, and cure

Transfer the required amount of Circalok 6410 A resin to a clean container and add Circalok 6410 B hardener at 17.5 parts resin to 10 parts hardener by weight. Mix until uniform without whipping excessive air into the material. Where entrapped air is present, evacuate the mixture before pouring.

  • Pour directly from the mixing container or use automatic meter/mix/dispense equipment.
  • Initial cure is 4 hours at 25°C or 1 hour at 65°C.
  • Complete cure is reached after one week at 25°C.
  • Cure time begins after the material reaches the stated temperature; account for oven ramp and part thermal mass.
Mixpac™ Dispensing Systems for Parker Lord Two Part Material

Mixpac™ Dispensing Systems for Parker Lord Two Part Material

Stage 1
Weigh
Measure 17.5 parts 6410 A resin and 10 parts 6410 B hardener by weight.
Stage 2
Mix and de-air
Mix to a uniform consistency while minimising air entrainment. Vacuum-de-air when necessary.
Stage 3
Pour or dispense
Apply within the 30-minute working life using direct pouring or validated meter/mix/dispense equipment.
Stage 4
Cure
Allow 4 hours at 25°C or 1 hour at 65°C for initial cure; full cure develops after one week at 25°C.

Storage and handling

Each component has a six-month shelf life when stored at 25°C in its original, unopened container. Before use, review the current product labels and applicable safety documentation. This material is for trained industrial or commercial personnel and is not intended for household or consumer application.

Final cured state

Flexible elastomer properties

The cured system is a soft, highly extensible polyurethane elastomer. These values are typical bulk-material properties and do not independently establish performance in a specific mould, encapsulated assembly, or loaded component.

Property Typical value Interpretation boundary
Hardness 55 Shore 00 Bulk cured-material hardness; it does not define load response in every geometry.
Tensile strength at 25°C 2.6 MPa (377 psi) Bulk tensile property, not a universal assembly strength.
Elongation at break 700% Tensile specimen property; it does not by itself establish fatigue, tear, or long-term dimensional performance.
Documented operating temperature -50°C to +105°C Use within the documented range still requires validation of the actual part, load, environment, and duty cycle.
Applications

Flexible casting for tooling, mechanical goods, and models

The published product scope is tooling, mechanical goods, and model making. Application-specific validation should address mould material, release strategy, section thickness, entrapped air, cure profile, mechanical loading, and operating environment.

Flexible polyurethane tooling or mould component cast with Circalok 6410

Tooling and mould components

Suitable for cast tooling elements and flexible mould-related parts where low mixed viscosity and a soft cured elastomer are relevant.

Flexible cast mechanical component made from black polyurethane elastomer

Mechanical goods

May be considered for flexible cast mechanical parts requiring high extension and the documented -50°C to +105°C operating range.

Prototype or scale model part cast from low-viscosity polyurethane

Model making and prototypes

Supports pouring into detailed model or prototype geometries, subject to adequate venting, de-airing, release preparation, and cure validation.

Evaluate Circalok™ 6410 for your casting process

Krayden can help review batch size, mix-ratio control, de-airing, mould geometry, dispensing equipment, cure profile, demould timing, and mechanical-property requirements for Circalok™ 6410 A/B.