CONATHANE EN-5317 Polyurethane Encapsulant

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

CONATHANE EN-5317 Polyurethane Encapsulant

Main features

  • 300 cP Mixed Viscosity
  • 1:1 Controlled Mixing
  • Clear Polyurethane for Potting and Bonding

Product Description

CONATHANE EN-5317 is an unfilled, two-component polyurethane system for potting, encapsulating, and bonding electrical and electronic assemblies. Part A urethane prepolymer and DP32127 Part B curative mix at 100:97 by weight or 1:1 by volume. The mixed system has a typical initial viscosity of 300 cP and a 10-15 minute work life at 25 C. Documented applications include electrical potting, electronic encapsulation, and adhesive bonding. Use either 7-10 days at 25 C or 16 hours at 80 C.

Key features

  • Flow and dispensing: Low initial mixed viscosity of 300 cP at 25 C.
  • Mix ratio: Cartridge-friendly 1:1 mix ratio by volume.
  • Application fit: Clear polyurethane for potting, encapsulation, and bonding.

Applications

  • Electrical potting
  • Electronic encapsulation
  • Adhesive bonding
Product Family

CONATHANE EN-5317

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Clear
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
2 Part
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
200 %

Additional Information

Potting compounds and encapsulants

CONATHANE EN-5317

CONATHANE EN-5317 is an unfilled, two-component polyurethane system for potting, encapsulating, and bonding electrical and electronic assemblies. Part A urethane prepolymer and DP32127 Part B curative mix at 100:97 by weight or 1:1 by volume. The mixed system has a typical initial viscosity of 300 cP and a 10-15 minute work life at 25 C.

Clear polyurethane1:1 by volume300 cP mixed viscosity10-15 min work life

CONATHANE EN-5317 - Two-component polyurethane potting and encapsulation system.

As-supplied and mixed properties

Component and mixed-system data

Part A, Part B, and mixed-state values are separated below.

Part A:Part B mix ratio
1:1 by volume
Equivalent to 100:97 by weight.
Typical initial viscosity
300 cP
Mixed system at 25 C.
State Property Value Unit Condition
Part A Viscosity 1,000 cP 25 C
Part A Specific gravity 1.06 None 25 C
Part B Viscosity 220 cP 25 C
Part B Specific gravity 1.03 None 25 C
Mixed system Mix ratio 100:97 By weight Part A:Part B
Mixed system Mix ratio 100:100 By volume Part A:Part B
Mixed system Initial viscosity 300 cP 25 C
Mixed system Work life 10-15 min 25 C
Processing

Mix, degas, dispense, and cure

Maintain the specified component ratio and processing conditions.

Mix ratio: 100:97 by weight or 1:1 by volume, Part A:DP32127 Part B.
Work life: 10-15 minutes at 25 C.
Cure options: 7-10 days at 25 C or 16 hours at 80 C.

Processing sequence for CONATHANE EN-5317.

Processing stages

Stage 1
Condition components
Mix each component before use. If Part A crystallizes, heat it to 60 C, mix thoroughly, and cool to room temperature.
Stage 2
Mix
Combine Part A and DP32127 Part B at 100:97 by weight or 1:1 by volume until homogeneous.
Stage 3
Degas and dispense
Degas at room temperature under more than 27 inHg vacuum, allowing container space for frothing, then dispense by hand, cartridge, meter-mix, or vacuum-potting methods.
Stage 4
Cure
Use either 7-10 days at 25 C or 16 hours at 80 C. Thin films reach tack-free condition in about 10 minutes at 80 C.
Protect components from moisture

Store sealed containers at 20-30 C in a dry environment away from direct sunlight. Shelf life is 12 months from shipment in the original sealed containers, while cartridge packaging may have a different shelf life. After opening, use immediately or blanket the container with dry air or nitrogen before resealing.

Final-state properties

Typical cured-system performance

Specimens for the physical-property data were cured for 16 hours at 80 C.

Property Value Unit Method or condition
Hardness 70 Shore A ASTM D2240 at 25 C
Tensile strength 2,200 psi ASTM D412 at 25 C
Ultimate elongation 200 % ASTM D412 at 25 C
Tear strength 110 pli ASTM D624 at 25 C
Linear shrinkage <0.1 % MIL-M-24041C
Lap shear, steel 775 psi Without primer
Lap shear, aluminum 310 psi Without primer
Thermal shock Pass, 10 cycles None MIL-I-16923E, -70 to 130 C

Values are typical and are not specification limits.

Applications

Electrical and electronic assembly protection

The clear polyurethane system supports potting, encapsulation, and adhesive use in assemblies exposed to heat, humidity, and sunlight.

Electrical potting
Low-viscosity filling around electrical components and connections.
Electronic encapsulation
Clear encapsulation for electronic assemblies operating in challenging environments.
Adhesive bonding
Bonding of electrical and electronic assembly components using the cured polyurethane system.
Next steps

Discuss CONATHANE EN-5317 with Krayden

Share your assembly geometry, dispense method, cure window, temperature exposure, and target properties to evaluate EN-5317 for potting, encapsulation, or bonding. Krayden can also help review the documented processing conditions and evaluation criteria before testing.