CONATHANE CE-1170

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

CONATHANE CE-1170

Main features

  • One-Component Acrylic Conformal Coating
  • 15-Minute Tack-Free Time
  • 2 x 10^15 ohm-cm Volume Resistivity

Product Description

CONAP® CE-1170 Acrylic Conformal Coating is a one-component, solvent-based acrylic conformal coating for printed circuit boards, epoxy-glass laminates, phenolic laminates, components, and other thin-film electronic applications. The coating is room-temperature or heat curable, with a typical tack-free time of 15 minutes, full cure in 24 hours at 25°C, or accelerated cure in 45 minutes at 60°C. It is documented as flexible, quick drying, repairable, humidity resistant, and hydrolytically stable, with a typical volume resistivity of 2 × 10¹⁵ ohm·cm.

Key features

  • One-component acrylic coating: The solvent-based material is used for thin-film protection of components and printed circuitry.
  • Fast handling: Typical tack-free time is 15 minutes, with room-temperature or accelerated heat cure.
  • Electrical insulation: Typical volume resistivity is 2 × 10¹⁵ ohm·cm.

Applications / Suitable for

  • Printed circuit boards and printed circuitry
  • Epoxy-glass and phenolic laminates
  • Thin-film coating of electronic components

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
400 mPa.s
General Properties
Appearance
Appearance at room temperature.
Amber, slight haze
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.95
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
13 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied or mixed-state values unless otherwise stated. These values are not sales specifications.

Property Value Unit Method / condition
Chemical base Acrylic N/A One-component solvent-based coating
Color Amber N/A One-gallon can configuration
Specific gravity 0.93 N/A As supplied
Viscosity 400 cP As supplied
Tack-free time 15 min Typical
Cure options 24 h at 25°C; 45 min at 60°C N/A Room-temperature or heat cure
Flash point 7 °C One-gallon can configuration

Leading Brands Trust in Our Products and Services