CONAP AD-1146-C

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

CONAP AD-1146-C

Main features

  • Lower-Viscosity Amber Adhesive-Primer Variant
  • Liquid-Polyurethane Bonding on Supported Substrates
  • Two-Coat Drying and Activation Process

Product Description

CONAP AD-1146-C Adhesive Primer is a distinct amber, lower-viscosity variant in the AD-1146 primer series for priming supported substrates before liquid-polyurethane bonding. The documented process uses two primer coats with controlled surface preparation, drying, and heat activation before the polyurethane is applied. The lower-viscosity AD-1146-C grade should remain distinct from AD-1146 during selection and processing. Applications are limited to the supported substrate and liquid-polyurethane bonding combinations documented for this exact variant.

Key features

  • Flow and dispensing: Distinct lower-viscosity amber AD-1146-series primer variant.
  • Application fit: Designed for priming supported substrates before liquid-polyurethane bonding.
  • Processing sequence: Two-coat application with controlled drying and heat activation.

Applications

  • Liquid-polyurethane bonding
  • Supported substrates
  • Variant-specific processes

Technical Specifications

General Properties
Color
The color
Amber
Solids
13-15 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
125-225 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
10 °C

Additional Information

SURFACE TREATMENT

CONAP AD-1146-C lower-viscosity adhesive primer

A distinct amber, lower-viscosity variant in the AD-1146 primer series. documented product information position AD-1146-C for priming supported substrates before liquid-polyurethane bonding and specify a two-coat application with controlled drying and activation before the polyurethane is applied. The variant is intended to keep the primer process distinct from the higher-viscosity AD-1146 grade.

Adhesive primerAmberLower viscosityTwo-coat process

AS-SUPPLIED PROPERTIES

Variant-specific product characteristics

Keep AD-1146-C properties and process controls separate from the related AD-1146 grades.

Property Value Condition
Product type Adhesive primer As supplied
Appearance Amber As supplied
Variant characteristic Lower viscosity than AD-1146 Series comparison
Bonding role Primer before liquid-polyurethane bonding Supported substrate systems

PROCESSING

Two-coat primer process

The two-coat AD-1146-C process uses controlled surface preparation, drying, activation, and polyurethane application.

  1. Prepare the supported substrate surface.
  2. Apply the first AD-1146-C primer coat.
  3. Dry or activate according to the controlled technical process.
  4. Apply the second primer coat and complete the documented drying / activation sequence before polyurethane application.

Process boundary

Do not substitute AD-1146 single-grade values or application instructions without confirming that they are explicitly stated for AD-1146-C.

TECHNICAL GUIDANCE

Maintain variant-specific process control

The lower-viscosity AD-1146-C grade should be evaluated on its own process record rather than treated as interchangeable with AD-1146.

Variant identity

Use the exact AD-1146-C designation in material, work-instruction and traceability records.

Coat sequence

Maintain the documented two-coat process and controlled drying / activation sequence.

System validation

Confirm the complete substrate, primer and liquid-polyurethane combination under the intended production conditions.

APPLICATIONS

Documented application context

AD-1146-C is documented for priming supported substrates before bonding with liquid polyurethane systems.

Liquid-polyurethane bonding

Use as a surface primer in documented liquid-polyurethane bonding systems.

Supported substrates

Apply only to substrate classes covered by the exact AD-1146-C technical record.

Variant-specific processes

Use where the lower-viscosity AD-1146-C variant and its two-coat process are appropriate to the controlled assembly.

Discuss your application with Krayden

For AD-1146-C evaluation, provide the substrate, surface preparation, polyurethane system and required application method so Krayden can help review the variant-specific two-coat primer process for your assembly. Krayden can also help review the documented processing conditions and evaluation criteria before testing.