CNP OM350

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

CNP OM350

Main features

  • Fine-feature no-clean solder paste with demonstrated Pin-in-Paste performance and robust solderability across OSP-Cu, Immersion Ag, Immersion Sn, ENIG, and lead-free HASL finishes.
  • Greater than 6-hour stencil life at 25 °C with stable storage and handling performance up to 30 °C for 21 days.
  • Halide-free ROL0 formulation with IPC Class III voiding performance and documented SIR and electromigration reliability results.

Product Description

ALPHA OM-350 Solder Paste is a lead-free, no-clean solder paste designed for fine-feature printing and demanding SMT reflow processes in air or nitrogen. Its broad reflow process window supports soldering on OSP-Cu, Immersion Ag, Immersion Sn, ENIG, and lead-free HASL surface finishes, including applications involving CSP and QFN components. ALPHA OM-350 combines stable paste viscosity with long stencil life and high tack force to support consistent printing and pick-and-place performance. The halide-free formulation is classified ROL0 according to IPC J-STD-004 and meets IPC Class III voiding performance.

Key features

  • Fine-feature and Pin-in-Paste capability: Supports fine-feature printing and demonstrated Pin-in-Paste performance for printing, dispensing, or pin-transfer SMT applications.
  • Long stencil life and stable viscosity: Provides greater than 6 hours of stencil life at 25 °C and stable handling up to 30 °C for 21 days.
  • Wide reflow process window: Supports straight-ramp and soak profiles in both air and nitrogen across multiple lead-free board finishes.
  • Controlled voiding and solder balling: Meets IPC Class III voiding performance and is formulated to reduce random solder ball levels.

Applications / Suitable for

  • Fine-feature SMT stencil printing
  • Pin-in-Paste / Paste-in-Hole assembly
  • High-density PWB assemblies
  • Assemblies using CSP and QFN components
Product Family

CNP OM350

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
SAC305; SACX Plus 0307; Innolot; Sn5/Pb92.5/Ag2.5

Additional Information

Technical properties

As-supplied / before-processing properties

Selected properties and available configurations of ALPHA OM-350 before reflow.

Property Value Method or condition
Available alloys SAC305, SACX Plus 0307, Innolot, 5Sn92.5Pb2.5Ag Other Sn-Ag-Cu alloys available upon request
Powder size Type 3, Type 4, Type 5 Available configurations
Flux residue Approximately 5% By weight
Flux classification ROL0 IPC J-STD-004
Halide content Halide free By titration and IC, IPC J-STD-004
Metal content - Type 4 89.0% M16 designation; Malcom Spiral Viscometer, JIS Z 3284 Annex 6
Metal content - Type 5 88.8% M16 designation; Malcom Spiral Viscometer, JIS Z 3284 Annex 6
Stencil life >6 hours 25 °C (77 °F)
Technical properties

After-processing / final-state properties

Selected electrical reliability and soldering performance results for ALPHA OM-350 under the stated test conditions.

Property Result Method or condition
IPC SIR Pass, 1.8 x 1010 ohms IPC J-STD-004; 168 hours at 85 °C/85% RH; pass >=1 x 108 ohm
Bellcore SIR Pass, 1.9 x 1012 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass >=1 x 1011 ohm
Electromigration Pass; initial 7.8 x 108 ohms, final 8.2 x 109 ohms Bellcore GR78-CORE; 10 V, 500 hours; pass = final > initial/10
HP ECM test Pass; no migration after 28 days 50 °C/90% RH, 5 V; Cu/ImmAg/ImmSn finishes; Hewlett-Packard EL-EN861-00
Copper corrosion Pass IPC J-STD-004 and JIS Z 3197:1986
Voiding performance Class III IPC voiding classification