BOSTIK L7132R

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK L7132R

Main features

  • Two-Component High-Green-Strength Laminating
  • Heat- and Creep-Resistant Bonding
  • Wide Vacuum-Form Processing Window

Product Description

Bostik 7132R / Boscodur® 4 is a two-component adhesive system developed for vacuum-form bonding of PVC films to wood, fiberboard, and other porous substrates. The system combines Bostik 7132R with Boscodur® 4 crosslinker to produce strong, heat- and creep-resistant bonds while providing excellent green strength for immediate edge trimming after removal from the vacuum former. The adhesive also exhibits excellent adhesion to polyolefin foams, polyester films, laminating films, foils, sheet metal, and cellulosic materials, making it suitable for demanding transportation, furniture, and industrial laminating applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Two-component adhesive system designed for vacuum-form laminating of PVC films.
  • Excellent green strength enables immediate edge trimming after vacuum forming.
  • Heat- and creep-resistant bond achieved through the Boscodur® 4 crosslinking system.
  • Wide processing window with excellent adhesion to vinyl, particle board, polyolefin foams, plastics, and cellulosic substrates.

Applications / Suitable For

  • Vacuum-form bonding of PVC films
  • Furniture decorative laminates
  • Automotive interior trim, door panels, dashboards and consoles
  • Aeronautic cabin interior laminates
  • Luggage shell construction

Technical Specifications

General Properties
Process Method
Two-component thermoset
Product Type
Material category or functional product class.
Two-component polyester adhesive
Thermal Properties
Operating Temperature
Vacuum forming: 43–99°C; cure up to 1 week °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property 7132R (Part A) Boscodur® 4 (Part B) Method / Condition
Appearance Amber liquid Brown liquid Typical physical property
Base Linear saturated polyester Polyisocyanate Supplier classification
Total solids 25.5% 68% Typical value
Viscosity 100 cP Thin liquid Brookfield LVF #1, 60 rpm, 25°C
Density 7.67 lb/gal 8.76 lb/gal Typical value
Flash point (SCC) 14°F (-10°C) 29°F (-2°C) Typical value
Solvent system MEK blend MEK Supplier description
Mix ratio 20–24 parts 7132R : 1 part Boscodur® 4 (by volume) Supplier recommendation
Shelf life 6 months at 55–80°F (15–27°C) Storage recommendation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Drying condition 80°C for 1–3 minutes — Circulating air oven
Vacuum lamination temperature 110–210°F (43–99°C) — Approximately 20 seconds or longer
Open pot life 8 hours — After mixing
Handling strength Immediate edge trimming after vacuum forming — Supplier description
Full cure Up to 72 hours to 1 week — Application dependent
Performance Heat- and creep-resistant bond with excellent edge-folding capability — Supplier description