BOSTIK L7132K

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

BOSTIK L7132K

Main features

  • Two-Part High-Green-Strength Laminating
  • Heat- and Creep-Resistant Bonding
  • BMS 5-127G Aerospace Qualification

Product Description

Bostik L7132K is a two-part solvent-based thermoset adhesive kit consisting of L7132R adhesive and Boscodur® 24T crosslinker. It is specifically formulated for vacuum and pressure bonding of PVC films to wood, fiberboard, and other porous substrates. The system provides excellent green strength for immediate edge trimming after vacuum forming and develops tough, heat- and creep-resistant bonds with excellent adhesion to vinyl, particle board, polyolefin foams, plastics, and other laminating materials. The product meets BMS 5-127G Type III Class 2 & 3 product specification requirements for aerospace applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Two-part thermoset adhesive system designed for vacuum and pressure laminating applications.
  • Excellent green strength allows immediate edge trimming after vacuum forming.
  • Heat- and creep-resistant bonds using the Boscodur® 24T crosslinking system.
  • Meets BMS 5-127G Type III Class 2 & 3 product specification for aerospace applications.

Applications / Suitable For

  • Vacuum-form bonding of PVC films
  • Aerospace interior decorative laminates
  • Automotive door panels, dashboards, consoles and interior trim
  • Decorative furniture laminates
  • PVC-coated luggage shell construction

Technical Specifications

General Properties
Process Method
Two-component thermoset
Product Type
Material category or functional product class.
Two-component thermoset laminating adhesive
Thermal Properties
Operating Temperature
Cure temperature: ≥88°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property L7132R (Part A) Boscodur® 24T (Part B) Method / Condition
Appearance Opaque liquid Dark brown liquid Typical physical property
Base Linear saturated polyester Polyisocyanate Supplier classification
Solvent system MEK blend MEK Supplier description
Total solids 25.5% 68% Typical value
Density @ 25°C 7.67 lb/gal (0.919 g/cm³) 8.76 lb/gal (1.05 g/cm³) Typical value
Viscosity 100 cP Thin liquid Brookfield
Flash point (SCC) 14°F (-10°C) 29°F (-2°C) Typical value
Mix ratio 16 parts L7132R : 1 part Boscodur® 24T (by volume) Supplier recommendation
Shelf life 9 months 55–80°F (15–27°C), unopened containers
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Wet adhesive application 100–150 g/m² Applied to least porous laminating surface
Lamination temperature 110–212 (41–100) °F (°C) Pressure lamination
Minimum cure temperature 190 (88) °F (°C) Minimum 4 minutes
Vacuum pressure Minimum 15 in Hg (51 kPa), 20 in Hg (68 kPa) preferred — Vacuum-form process
Pot life 8 hours After mixing
Performance Tough, heat- and creep-resistant bond with immediate edge trimming capability — Supplier description