BOSTIK L1096MR

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

BOSTIK L1096MR

Main features

  • One- or Two-Component Contact Adhesive
  • Fast Tack and Heat Resistance
  • Multi-Substrate Brush/Knife/Roll-Coat Application

Product Description

Bostik LIQ. 1096MR is a general-purpose solvent-based contact adhesive designed for laminating, rubber gasket installation, and self-bonding of chloroprene and SBR rubber. It can be used as either a one-component or two-component system with Boscodur® 4L curative, providing fast tack, rapid strength development, tough flexible bond films, and good heat resistance. The adhesive is suitable for bonding high-pressure laminates to wood, particleboard, or metal, as well as a variety of rubber and rigid plastic substrates. :contentReference[oaicite:0]{index=0}

Key Features

  • Versatile contact adhesive that can be used as either a one-component or two-component system.
  • Fast tack and rapid strength development for efficient industrial assembly and laminating processes.
  • Tough, flexible bond films with good heat resistance and adhesion to a wide variety of substrates.
  • Compatible with Boscodur® 4L curative for enhanced performance when used as a two-part system.

Applications / Suitable For

  • High-pressure laminate bonding
  • Rubber gasket installation
  • Self-bonding of chloroprene rubber
  • Self-bonding of SBR rubber
  • Bonding wood, particleboard and metal
  • General rubber and rigid plastic bonding

Technical Specifications

General Properties
Process Method
Solvent evaporation (optional Boscodur® 4L crosslinking)
Product Type
Material category or functional product class.
Solvent-based contact adhesive
Thermal Properties
Operating Temperature
Heat activation: 71–93°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Product type General-purpose solvent-based contact adhesive — Supplier classification
Appearance Amber liquid — Typical physical property
Total solids 24.5 % Typical physical property
Viscosity 1,100 cP Typical physical property
Density 7.24 lb/gal (0.87 g/cc) — Typical physical property
Flash point 32 °F Typical physical property
Shelf life Approximately 270 days (9 months) — Typical storage condition
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Bond characteristics Tough, flexible film — Supplier description
Strength development Fast — Supplier description
Heat resistance Good — Supplier description
Heat activation temperature 160–200 (71–93) °F (°C) Supplier recommendation
Two-part mix ratio 100:5 By weight LIQ. 1096MR : Boscodur® 4L
Mixed pot life 6–8 hours When mixed with Boscodur® 4L