BOSTIK 70-05A

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BOSTIK 70-05A

Main features

  • High-Strength Structural SMP Bonding
  • Primerless Multi-Substrate Adhesion
  • UV and Weather Resistance

Product Description

Bostik 70-05A is a one-component, moisture-curing adhesive and sealant based on Silyl Modified Polymer (SMP) technology. Developed for high-strength elastic structural joints, it provides higher green strength and higher tensile strength than Bostik 70-01A and 70-03A while maintaining permanent elasticity. The solvent-, isocyanate-, and PVC-free formulation delivers primerless adhesion on many substrates, excellent UV and weather resistance, and durable performance for transportation and industrial assembly applications.

Key Features

  • High-strength SMP adhesive with increased green strength and tensile strength for structural bonding applications.
  • Primerless adhesion to many metals, glass, polyester, PVC, and painted or lacquered wood when properly prepared.
  • Permanent elasticity with excellent UV and weather resistance from -40°C to 120°C.
  • Fast processing with approximately 10-minute skin-forming time and less than 15-minute open time.

Applications / Suitable For

  • Trim bonding
  • Panel bonding
  • Floor bonding
  • Bus, caravan, train and truck assembly
  • Roof bonding
  • Aluminum and polyester corner profile bonding
  • Bonding polyester components to metal frames

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
High-strength SMP adhesive & sealant
Thermal Properties
Operating Temperature
-40°C to +120°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Basic material Silyl Modified Polymer (SMP) — Supplier classification
Curing method Moisture cure — One-component system
Specific gravity Approx. 1.5 g/mL Typical value
Skin-forming time Approx. 10 minutes 20°C / 50% RH
Open time <15 minutes 20°C / 50% RH
Curing speed after 24 hours 3 (0.125) mm (in.) 20°C / 50% RH
Green strength 500 Pa Physical Rheometer MC100
Application temperature 5–35 (41–95) °C (°F) Recommended application range
Shelf life 12 months (18 months for cartridges) — Stored unopened at 5–30°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness Approx. 60 Shore A DIN 53505
Volume change <3 % DIN 52451
Tensile stress (100%) 2.7 (390) MPa (psi) DIN 53504 / ISO 37
Tensile stress at break 3.5 (500) MPa (psi) DIN 53504 / ISO 37
Elongation at break 200 % DIN 53504 / ISO 37
Shear stress 3.0 (435) MPa (psi) DIN 53283 / ASTM D1002
Tear propagation Approx. 17 N/mm Typical value
E-Modulus (10%) 4.8 (700) MPa (psi) Typical value
Temperature resistance -40 to 120 (-40 to 248) °C (°F) Continuous service
Short-term temperature resistance 180 (356) °C (°F) Maximum 30 minutes
UV & weather resistance Excellent — Supplier classification