BOSTIK 70-03A

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BOSTIK 70-03A

Main features

  • 2.5 MPa Lap Shear
  • Primerless Multi-Substrate Adhesion
  • Up to 120 deg C Service

Product Description

Bostik 70-03A is a one-component, moisture-curing adhesive and sealant based on Silyl Modified Polymer technology. It is designed for high-strength elastic construction joints and general bonding and sealing applications. The solvent-, isocyanate-, and PVC-free formulation combines high green strength, low residual tack, primerless adhesion on many substrates, and excellent UV and weather resistance. It remains permanently elastic from -40°C to 100°C and is compatible with most industrial paint and lacquer systems, subject to compatibility testing.

Key Features

  • High-strength elastic bonding: Provides approximately 2.5 MPa lap shear strength and 250% elongation at break.
  • Primerless adhesion: Adheres to many metals, glass, PVC, polyester, and painted or lacquered wood when surfaces are properly prepared.
  • Durable environmental performance: Offers excellent UV and weather resistance with temperature resistance from -40°C to 120°C.
  • Fast processing: Provides a 10-minute skin-forming time and less than 15 minutes of open time at 20°C and 50% relative humidity.

Applications / Suitable for

  • Sunroof assemblies
  • Composite assembly
  • Elastic bonding and sealing in buses, caravans, trains, and trucks
  • Bonding vehicle roofs, floor systems, corner profiles, and polyester components
  • Sealing welded seams

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
SMP adhesive & sealant
Thermal Properties
Operating Temperature
-40°C to +120°C °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Basic material Silyl Modified Polymer — Supplier classification
Curing method Moisture cure — One-component system
Specific gravity Approx. 1.4 g/mL Typical value
Skin-forming time 10 minutes 20°C and 50% RH
Open time <15 minutes 20°C and 50% RH
Curing speed after 24 hours 3 (0.125) mm (in.) Typical value
Green strength 300 Pa Physical Rheometer MC100
Application temperature 5 to 35 (40 to 95) °C (°F) Supplier recommended range
Shelf life 18 months for cartridges; 12 months for sausages — Unopened packaging stored dry at 5°C to 30°C
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Shore A hardness Approx. 55 Shore A Typical cured property
Volume change <3 % Typical cured property
Tensile stress at 100% elongation 2.3 (245) MPa (psi) Typical cured property
Tensile stress at break 2.6 (275) MPa (psi) Typical cured property
Elongation at break 250 % Typical cured property
Lap shear strength 2.5 (360) MPa (psi) Typical cured property
E-modulus at 10% 3.3 (475) MPa (psi) Typical cured property
Temperature resistance -40 to 120 (-40 to 250) °C (°F) Continuous resistance
Short-term temperature resistance 180 (350) °C (°F) Maximum 30 minutes
UV and weather resistance Excellent — Supplier classification