BONDERITE S-OT 310B

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

BONDERITE S-OT 310B

Main features

  • PTFE Dry-Film Low-Friction Lubrication
  • Oil, Solvent, and Chemical Resistance
  • Metal and Rubber Coating Process

Product Description

BONDERITE® S-OT 310B ACHESON is a two-package resin-bonded dry film lubricant formulated as a PTFE dispersion in a solvent/water system. When combined with BONDERITE® L-GP T A COMP ACHESON, it forms a fluorocarbon coating in a thermosetting binder that delivers low-friction, stick-slip-free performance for metal and rubber substrates. The spray-applied coating provides durable lubrication and chemical resistance for industrial and consumer applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Two-package PTFE dry film lubricant for durable low-friction coatings.
  • Produces stick-slip-free fluorocarbon coatings after curing.
  • Suitable for metal and rubber substrates.
  • Excellent resistance to oils, alcohols, ketones, dilute acids, esters, and aromatic hydrocarbons.
  • One-component base mixed immediately before use with BONDERITE® L-GP T A COMP ACHESON.

Applications / Suitable for

  • Metal components
  • Rubber components
  • Industrial mechanical assemblies
  • Consumer product components
  • Spray-applied dry film lubrication

Technical Specifications

General Properties
Product Type
Material category or functional product class.
wo-component PTFE coating

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Lubricant — Supplier classification
Product type PTFE dispersion in solvent/water — Supplier description
Application Dry film lubricant — Supplier classification
Pigment None — Wet product
Binder Thermosetting resin — Wet product
Solids content ~10.5 % Wet product
Color Blue — Wet product
Flash point 8 °C Wet product
Density 910 kg/m³ Wet product
Theoretical coverage 7.7 m²/kg @ 10 µm dry film thickness
Recommended storage temperature 5–30 °C Unopened container
Shelf life 18 months Unopened original packaging
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Coating color Green — Cured coating
Coefficient of friction (static & kinetic) ~0.06 — Cured coating
Recommended dry film thickness (metal) 10–25 µm Typical application
Recommended dry film thickness (rubber) 5–10 µm Typical application
Continuous service temperature 150 °C Cured coating
Intermittent service temperature 160 °C Cured coating
Chemical resistance Resistant to oils, alcohols, ketones, chlorinated hydrocarbons, dilute acids, esters, aromatic hydrocarbons and gasohol — Cured coating
Curing schedule 160°C / 60 min
180°C / 30 min
200°C / 10 min
— Substrate temperature

Leading Brands Trust in Our Products and Services