BONDERITE M-CR 1200S

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BONDERITE M-CR 1200S

Main features

  • MIL-DTL-5541 Qualified Aluminum Coating
  • Immersion, Spray, or Brush Application Flexibility
  • Wide-Range Bath Operating Window

Product Description

BONDERITE M-CR 1200S AERO is a brown powdered chromate conversion-coating chemical used to treat aluminum and its alloys. Mixed into an aqueous bath and applied by immersion, spray, or brush, it forms a light iridescent golden-to-tan coating that reduces corrosion and improves paint adhesion. The bath operates at a pH of 1.3 to 2.1 and a temperature of 20 to 35 deg C (68 to 95 deg F), with a contact time of 15 seconds to 3 minutes. Immersion or spray baths are built up at 6.3 lb per 100 gallons, while brush-application baths use 12.5 lb per 100 gallons. The coating chemical is listed on Qualified Product List QPL-81706 as an approved material for Class 1A and Class 3 coatings, bare or painted, in accordance with MIL-DTL-5541.

Key features

  • Immersion, Spray, or Brush Application: applied to aluminum by immersion, spray, or brush depending on process needs
  • MIL-DTL-5541 Qualified Coating: listed on QPL-81706 as an approved material for Class 1A and Class 3 coatings
  • Wide Operating pH and Temperature Range: bath operates at pH 1.3 to 2.1 and 20 to 35 deg C (68 to 95 deg F)

Applications

Chromate conversion coating of aluminum before painting or for corrosion-protection processes.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
brown powder

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceBrown powder-As supplied
Bath pH1.3 to 2.1pHOperation and control; optimum 1.3 to 1.8
Operating temperature20 to 35 (68 to 95)deg C (deg F)Immersion, spray, or brush bath
Contact time15 to 180secImmersion, spray, or brush application
Bath makeup, immersion or spray6.3lb per 100 galChemical / bath preparation
Bath makeup, brush12.5lb per 100 galChemical / bath preparation