BONDERITE L-FG LS 2127

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

BONDERITE L-FG LS2127

Main features

  • Up to 1649 deg C Service
  • Anti-Stick Non-Ferrous Tooling Coating
  • Brush, Spray, or Dip Application

Product Description

BONDERITE L-GP LS 2127 ACHESON (formerly known as ACHESON LS-2127) is a boron nitride-based protective coating formulated for high-temperature processing of non-ferrous metals. It functions as a mold release, anti-stick agent, and precoat lubricant for demanding thermal processes, helping improve die and mold life while preventing adhesion of non-ferrous alloys to coated surfaces. The water-based coating can be applied by brushing, dipping, or spraying after appropriate dilution, making it suitable for a variety of industrial high-temperature applications.

Key Features:

  • High-temperature mold release for non-ferrous metals up to 1649°C (3000°F).
  • Anti-stick protective coating for high-temperature processing applications.
  • Non-reactive boron nitride formulation with fine particle size.
  • Helps increase die life and mold life cycles.
  • Can be applied by brush, dip, or spray using water dilution as required.

Applications / Suitable For:

  • Isothermal forming die lubricant and precoat.
  • Laser drilling operations.
  • Brazing protective coating.
  • Welding protective coating.

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Boron nitride protective coating
Thermal Properties
Operating Temperature
Up to 1649°C (3000°F) °C

Additional Information

Property Value
Appearance White fluid
Solids 30%
Viscosity 700–800 cP
Density 10 lb/gal
pH 10–12
Diluent Water
Shelf Life 12 months from date of qualification under original seal
Storage Do not store below 0°C (32°F) or near furnaces or high-temperature environments.
Property Value
Maximum Service Temperature Up to 1649°C (3000°F) for non-ferrous metal mold release applications
Primary Function High-temperature mold release and anti-stick protective coating
Surface Performance Non-ferrous alloys will not adhere to boron nitride coating
Tooling Benefit Helps increase die life and mold life cycles