BONDERITE C-SO 2382

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-SO 2382

Main features

  • Aerospace NESHAP/AQMD Solvent Compliance
  • Fast-Evaporating Residue-Free Surface Prep
  • Noncorrosive Ferrous/Nonferrous Metal Cleaning

Product Description

BONDERITE C-SO 2382-BK AERO (formerly known as TURCO 4460-BK) is a low composite vapor pressure solvent formulated as an alternative to methyl ethyl ketone (MEK) and similar high-vapor-pressure solvents. It is supplied as a water-white liquid for hand-wipe cleaning of metal surfaces prior to painting or bonding and for cleaning bearings, instruments, and electronic components. The solvent evaporates rapidly, leaves no surface residue after evaporation, is noncorrosive to ferrous and nonferrous metals, and provides excellent solvency for oily soils and paint residues while meeting aerospace VOC compliance requirements.

Key Features:

  • Low composite vapor pressure solvent for aerospace cleaning applications.
  • Rapid evaporation with no surface residue after drying.
  • Noncorrosive to ferrous and nonferrous metals.
  • Excellent solvency for oily soils and paint residues.
  • NESHAP compliant and meets South Coast AQMD Rule 1124 composite vapor pressure requirements.

Applications / Suitable For:

  • Hand-wipe cleaning of metal surfaces prior to painting or bonding.
  • Cleaning bearings, instruments, and electronic components.

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Low composite vapor pressure solvent cleaner
Thermal Properties
Operating Temperature
Ambient use °C

Additional Information

Property Value
Appearance Water-white liquid
Product Type Low composite vapor pressure solvent
Recommended Use Use at full strength
VOC 815 g/L
Composite Vapor Pressure 37 mm Hg (Rule 1124)
Property Value
Residue After Evaporation Does not leave surface residue after evaporation
Evaporation Behavior Evaporates rapidly from surfaces
Metal Compatibility Noncorrosive to ferrous and nonferrous metals
Cleaning Performance Excellent solvency for oily soils and paint residues