BIOACT EC-7R

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT EC-7R

Main features

  • 99% USDA-Certified Biobased Cleaner
  • Broad Electronics Residue Removal
  • Water-Rinsable Ambient Processing

Product Description

BIOACT EC-7R is a USDA Certified Biobased Product (99%) and high-performance electronics cleaner for semi-aqueous spray and immersion defluxing. The citrus-terpene-based cleaner is water rinsable and separates from water in the rinse section, supporting solvent recovery and recycling. Used at full concentration and ambient temperature, BIOACT EC-7R removes lead-free, no-clean, RMA, and HMP flux residues, fingerprint oils, ionic contamination, and uncured SMD adhesives. It provides a Kauri-Butanol value of 95, low viscosity, high soil loading, and compatibility with commercially available immersion and spray-under-immersion cleaning equipment.

Key features

  • USDA Certified Biobased Product: Certified biobased content of 99%.
  • Broad defluxing performance: Removes lead-free, no-clean, RMA, and HMP flux residues.
  • Ionic and process-soil removal: Removes ionic contamination, fingerprint oils, and uncured SMD adhesives.
  • Ambient full-strength processing: Used without dilution for manual and immersion cleaning; heat is not recommended.
  • Water rinsing and solvent separation: Separates from rinse water to support solvent recovery and recycling.
  • High solvency and low viscosity: Kauri-Butanol value of 95 and viscosity of 0.8 cP.

Applications / Suitable for

  • Semi-aqueous spray and immersion defluxing
  • Removal of lead-free, no-clean, RMA, and HMP flux residues
  • Removal of ionic contamination and fingerprint oils
  • Manual cleaning and removal of uncured SMD adhesives
Product Family

BIOACT EC-7R

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
47 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
0.8 mPa.s
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.84
Vapor Pressure
<2 mmHg

Additional Information

Surface Treatments | Electronics Cleaner & Defluxer

BIOACT EC-7R

BIOACT EC-7R is a USDA Certified Biobased Product (99%) for semi-aqueous electronics defluxing. The water-rinsable citrus-terpene cleaner removes multiple flux-residue types, ionic contamination, fingerprint oils, and uncured SMD adhesives at ambient temperature and separates from rinse water for recovery and recycling.

99% certified biobased KB value 95 0.8 cP viscosity 47°C flash point Ambient full-strength use

Vantage Can

Product data

As-Supplied Properties

Typical product data for evaluation. These values are not guaranteed specifications.

Property Value Unit Method / condition
Physical state Liquid — As supplied
Appearance Clear, light yellow — As supplied
Odor Mild citrus — As supplied
Flash point 47 (117) °C (°F) Closed cup
Viscosity 0.8 cP 25°C
Specific gravity 0.84 — 25°C
Vapor pressure <2.0 mmHg 20°C
Kauri-Butanol value 95 — Typical solvency value
Application

Cleaning and Rinse Process

Use BIOACT EC-7R at full concentration and ambient temperature. Select manual, immersion, or spray-under-immersion equipment according to the assembly, flux type, soil loading, and required rinsing and cleanliness controls.

Concentration: Use at full concentration for manual and immersion cleaning.
Temperature: Use at ambient temperature; heating the immersion wash bath is not recommended.
Equipment: Suitable for manual application, immersion equipment, and spray-under-immersion systems.

 

Defluxing Sequence

Stage 1
Apply the cleaner
Apply BIOACT EC-7R at full concentration by brush, pad, or cloth, or charge the immersion cleaning reservoir with full-strength product.
Stage 2
Remove flux and process soils
Process at ambient temperature to remove supported lead-free, no-clean, RMA, and HMP flux residues, fingerprint oils, ionic contamination, and uncured SMD adhesives.
Stage 3
Water rinse and separate
Rinse the cleaned assembly with water. BIOACT EC-7R separates from water in the rinse section, supporting solvent recovery and recycling within a controlled process.
Storage and Handling

Store BIOACT EC-7R in its original, sealed container above 50°F (10°C). The documented shelf life is 36 months under these conditions. Standard packages include 35 lb (16 kg) pails and 390 lb (177 kg) drums. Keep containers tightly closed in a cool, well-ventilated area away from heat, sparks, flames, and incompatible strong acids or oxidizing agents. Use appropriate ventilation and personal protective equipment and consult the current SDS for complete handling, storage, transport, and disposal requirements.

Environmental and Certification Profile

Issue or observation Source-supported guidance Qualification boundary
USDA Certified Biobased Product 99% Certified biobased content shown on the product technical data sheet.
Ozone depletion potential Zero Supplier-reported product environmental profile.
Global warming potential Low Supplier-reported qualitative classification.
Volatile organic compound 838 g/L Confirm current regional and process-specific VOC requirements.
Hazardous air pollutant No Supplier-reported product status.
SARA / NESHAPs Not regulated Confirm current jurisdictional, facility, and process applicability.
RCRA Not regulated Supplier TDS status; spent-material classification depends on contamination and jurisdiction.

Defluxing and Cleaning Guidance

Supported flux and process soils
BIOACT EC-7R removes lead-free, no-clean, RMA, and HMP flux residues, fingerprint oils, ionic contamination, and uncured SMD adhesives. Confirm the actual flux chemistry, cure condition, assembly materials, and cleanliness endpoint under production conditions.
Water rinsing, soil loading, and recovery
The cleaner is water rinsable, supports high soil loading, and separates from water in the rinse section. Establish bath control, rinse-water management, phase separation, solvent recovery, and disposal practices for the specific cleaning system.
Supported use contexts

Applications

BIOACT EC-7R supports semi-aqueous electronics cleaning where flux residues, ionic contamination, fingerprint oils, or uncured SMD adhesives must be removed from compatible assemblies using ambient manual or equipment-based processes.

Immersion defluxing
Use full-strength product at ambient temperature in commercially available immersion equipment for supported lead-free, no-clean, RMA, and HMP flux residues.
Spray-under-immersion cleaning
Use in compatible spray-under-immersion equipment for semi-aqueous defluxing, followed by controlled water rinsing and solvent separation.
Manual electronics cleaning
Apply full-strength cleaner by brush, pad, or cloth for localized removal of flux residues, fingerprint oils, ionic contamination, and uncured SMD adhesive.
Next steps

Technical Support

Work with Krayden to evaluate BIOACT EC-7R against your flux chemistry, assembly materials, ionic-cleanliness target, cleaning equipment, rinse configuration, and solvent-recovery process. Our team can help review compatibility, process conditions, packaging, sampling, and implementation requirements.

Leading Brands Trust in Our Products and Services