ARALDITE AW139

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AW139

Main features

  • Two-Component Room-Temperature Epoxy
  • High-Temperature Chemical Resistance
  • Multi-Material Metal/Composite/Electronics Bonding

Product Description

ARALDITE® AW 139-1 / Hardener HW 5323-1 is a two-component, room-temperature-curing epoxy paste adhesive for structural bonding where elevated temperatures or aggressive service environments may be encountered. The thixotropic, non-sagging mixed adhesive fills gaps up to 5 mm and is suitable for bonding metals, electronic components, GRP structures, and other supported assemblies. A 100:50 mix ratio by weight or volume, approximately 110-minute pot life at 25°C, and specified lap shear strength above 14 MPa at 25°C provide a practical balance of application control and bonded-joint performance.

Key features

  • Environmental resistance: Resistant to water and a wide variety of chemicals.
  • Gap-filling paste: Thixotropic, non-sagging consistency supports gaps up to 5 mm.
  • Controlled working time: Approximately 110-minute pot life for a 100 g mixed mass at 25°C.

Applications / Suitable for

  • Structural bonding of metals
  • Bonding electronic components
  • GRP structures and assemblies exposed to demanding environments

Technical Specifications

General Properties
Color
The color
Beige
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.6
Physical Properties
Viscosity (Part A)
65 mPa.s
Electrical Properties
Dielectric Strength
Dielectric strength is measured in kV per mm and is calculated by the Breakdown voltage divided by the thickness of the tested material. Those two properties go hand in hand and while Breakdown voltage is always thickness dependent, dielectric strength is a general material property. As an example, the dielectric strength of Polyimide is 236 kV/mm. If we place 1mm of Polyimide between two electrodes, it will act as an insulator until the voltage between the electrodes reaches 236 kV. At this point it will start acting as a good conductor, causing sparks, potential punctures and current flow.
25 kV/mm
Surface Resistivity
46000000000000000 Ohms/sq
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
2700000000000000 Ohms⋅cm

Additional Information

Technical properties

Before-mixing properties

Individual component properties before ARALDITE® AW 139-1 and Hardener HW 5323-1 are combined.

Property ARALDITE® AW 139-1 Hardener HW 5323-1
Color and form Beige paste Grey paste
Specific gravity Approx. 1.6 Approx. 1.5
Viscosity at 25°C 50–80 Pa·s Thixotropic
Mix ratio 100 parts AW 139-1 to 50 parts HW 5323-1 by weight or volume
Technical properties

After-mixing properties

Properties of the mixed adhesive before cure.

Property Value Condition
Color and form Grey paste Mixed adhesive
Specific gravity Approx. 1.6 Mixed adhesive
Rheology Thixotropic Non-sagging paste
Pot life 110 minutes 100 g mixed mass at 25°C
Gap-filling capability Up to 5 mm Non-sag application

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers