ARALDITE AW134

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE AW134

Main features

  • Controlled Paste-Grade Resin Handling
  • 80-to-100-Minute System Pot Life
  • Multipurpose Metal and Ceramic Bonding

Product Description

ARALDITE AW 134 Epoxy Resin is a white-to-beige paste resin component for a two-part, room-temperature-curing epoxy adhesive system used with ARADUR HY 991. The resin has a typical specific gravity of 1.2 to 1.3 and viscosity of 20 to 40 Pa s. The complete system mixes at 100:30 by weight or 100:40 by volume and provides a typical 80-to-100-minute pot life for 100 g at 25 deg C. When combined with the specified hardener, it forms a solvent-free multipurpose adhesive for bonding metals, ceramics, and other common substrates. Cured-joint properties belong to the complete AW 134/HY 991 formulation and cure.

Key features

  • Paste-grade resin handling: The AW 134 component has a typical viscosity of 20 to 40 Pa s.
  • Extended mixed working window: The AW 134/HY 991 system provides a typical 80-to-100-minute pot life at 25 deg C.
  • Room-temperature epoxy system: The specified resin and hardener form a solvent-free adhesive that cures at room temperature.

Applications

Bonding metals, ceramics, and other common substrates within the specified AW 134/HY 991 adhesive system.

Technical Specifications

General Properties
Color
The color
white to beige paste
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:30 by weight
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.2-1.3

Additional Information

Technical properties

As-supplied / before-processing properties

AW 134 component values are separated from mixed AW 134/HY 991 system data.

PropertyValueUnitMethod / condition
AW 134 appearanceWhite to beige paste-Visual; typical
AW 134 specific gravity1.2 to 1.3-Typical
AW 134 viscosity20 to 40Pa sTypical
System mix ratio100:30 by weight; 100:40 by volumepartsAW 134 resin to HY 991 hardener
Mixed pot life80 to 100min100 g at 25 deg C; typical