ARALDITE 2042

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ARALDITE 2042

Main features

  • One-Hour Room-Temperature Handling
  • Convenient 1:1 Volume Mixing
  • High-Elongation Flexible Bonding

Product Description

ARALDITE 2042 A/B Adhesive is a two-part, rapid-curing polyurethane adhesive for bonding selected plastics and assemblies with dissimilar coefficients of thermal expansion. The resin and hardener mix at 80:100 by weight or 1:1 by volume to form a pink adhesive with a typical three-minute pot life at 25 deg C for a 4 fl oz batch. Typical handling strength is reached in one hour at 25 deg C, while elevated-temperature schedules shorten handling time. The cured adhesive combines 250% tensile elongation with tested lap-shear performance on aluminum and Metton specimens, supporting flexible structural bonding where joint movement and impact resistance matter.

Key features

  • Rapid handling schedule: Typical handling strength develops in one hour at 25 deg C and faster with the listed heat-cure schedules.
  • Convenient volume mixing: A 1:1 resin-to-hardener volume ratio supports controlled preparation.
  • Flexible cured profile: Typical tensile elongation reaches 250% after the stated cure.

Applications

Bonding selected polycarbonate, ABS, nylon, and Metton substrates, plus assemblies with dissimilar coefficients of thermal expansion.

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
3 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system values; resin, hardener, and mixed states are identified separately.

PropertyValueUnitMethod / condition
AppearancePart A: white; Part B: red; mixed: pink-Visual; typical
DensityPart A: 1.10; Part B: 1.30; mixed: 1.20g/cm^3ASTM D792; typical
ViscosityPart A: 50,000; Part B: 20,000; mixed: 50,000cPASTM D2393; 25 deg C; typical
Mixed pot life3minASTM D2471; 25 deg C; 4 fl oz batch; typical
Mix ratio, A:B80:100 by weight; 100:100 by volumepartsResin to hardener
Technical properties

After-processing / final-state properties

Typical cured-system values. Standard lap-joint specimens were cured for 20 minutes at 100 deg C unless otherwise stated.

PropertyValueUnitMethod / condition
Tensile lap-shear strengthAluminum: 1,450 (10); Metton: 800 (5.5)psi (MPa)ASTM D1002; tested configuration
Coefficient of thermal expansionBelow Tg: 13.5 x 10^-5; above Tg: 23 x 10^-5in/in/deg CASTM E831; typical
Glass-transition temperature86 (30)deg F (deg C)ASTM D4065; typical
Elongation at tensile break250%ASTM D638; typical
Ultimate tensile strength2,100 (14.5)psi (MPa)ASTM D638; typical
Hardness85Shore DASTM D2240; typical