ARALDITE 2022-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 2022-1

Main features

  • 1 MPa Lap Shear
  • Thixotropic Gap-Filling Control
  • Multi-Substrate Bonding Capability

Product Description

ARALDITE 2022-1 is a two-component, room-temperature-curing, toughened methacrylate structural adhesive for fast assembly on a wide range of substrates, including materials that can be difficult to bond. Supplied at a 1:1 mix ratio by weight and volume, it forms a pale-yellow, thixotropic adhesive with a typical pot life of approximately 10 minutes at 25°C. The system combines rapid lap-shear strength development with gap-filling capability up to 4 mm and can be used effectively with limited surface preparation, although clean, mechanically abraded or chemically etched surfaces provide the strongest and most durable joints.

Key features

  • Fast strength development: Typical lap shear strength exceeds 1 MPa after 12 minutes and 10 MPa after 17 minutes at 23°C.
  • Controlled 1:1 processing: The mixed adhesive is thixotropic, has a typical 10-minute pot life at 25°C, and is available for cartridge mixing and dispensing.
  • Gap-filling multi-substrate bonding: Supports gaps up to 4 mm and is intended for a wide range of metal, plastic, and composite substrates.

Applications / Suitable for

  • Fast room-temperature assembly operations
  • Bonding evaluated metals, plastics, and fiber-reinforced composites
  • Joints requiring gap filling or tolerance of less-than-ideal pretreatment

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
10 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1
Physical Properties
Viscosity (Part A)
32000 mPa.s
Viscosity (Part B)
30000 mPa.s

Additional Information

Technical properties

As-supplied and mixed properties

Component and mixed-adhesive properties. Values identified as approximate or typical are informational and are not guaranteed specifications.

Property Value Unit Method / condition
Adhesive system Two-component toughened methacrylate — Room-temperature-curing structural adhesive
Color Part A: off-white; Part B: yellow; mixed: pale yellow — Visual
Specific gravity Part A: 1.02; Part B: 0.96; mixed: ca. 1 — As supplied
Viscosity at 25°C Part A: 15-50; Part B: 10-50; mixed: thixotropic Pa·s A191 for component viscosity
Mix ratio, A:B 100:100 by weight and 100:100 by volume parts Equivalent to 1:1 by weight and volume
Pot life ca. 10 min 100 g at 25°C
Time to peak exotherm 15-30 min 20 g; A159
Gap-filling capability Up to 4 mm Documented maximum gap-filling capability
Storage and Handling

Store ARALDITE 2022-1 for up to 18 months at 2-8°C in the original sealed containers. The product may be brought to room temperature before use, but total room-temperature exposure should not exceed six months, and long-term exposure above 25°C reduces shelf life. Clean tools with hot water and soap before adhesive residue cures. Consult the current Safety Data Sheet before handling.

Cured adhesive

Typical tensile properties

Typical average values for specimens cured for 16 hours at 40°C and tested at 23°C. These laboratory values are not guaranteed specifications or universal joint design values.

Property Value Unit Method / condition
Tensile strength 45 MPa ISO 527; cured 16 h at 40°C and tested at 23°C; typical average value
Tensile modulus 1700 MPa ISO 527; cured 16 h at 40°C and tested at 23°C; typical average value
Elongation at break >5 % ISO 527; cured 16 h at 40°C and tested at 23°C; typical average value

Bonding and environmental performance evidence

ARALDITE 2022-1 has been evaluated in substrate-specific and environmental laboratory tests. Results apply to the stated materials, preparation, cure schedule, and test conditions and should not be treated as universal design allowables.

Metal-to-metal lap-shear evaluation
ISO 4587 lap-shear testing covers aluminum L165, steel 37/11, stainless steel V4A, galvanized steel, copper, and brass.
Cured 16 h at 40°C and tested at 23°C after sandblasting and degreasing. Steel and stainless-steel tests used a 0.25 mm adhesive joint.
Plastic and composite lap-shear evaluation
EP-GRP, UP-GRP, CFRP, SMC, ABS, PVC, PMMA, polycarbonate, and polyamide were evaluated. Substrate failure was observed for EP-GRP, UP-GRP, SMC, ABS, PVC, PMMA, and polycarbonate under the stated test conditions.
ISO 4587; cured 16 h at 40°C and tested at 23°C after light abrasion and isopropanol degreasing.
Thermal cycling on aluminum
A typical lap-shear strength of 27 MPa was measured after 100 thermal cycles from -30°C to 70°C.
ISO 4587 on aluminum; sandblasted and degreased; cured 16 h at 40°C. Each 6 h cycle used 2 h at -30°C, a 1 h ramp to 70°C, 2 h at 70°C, and a 1 h ramp to -30°C.
Environmental and temperature test coverage
Additional lap-shear evaluations cover immersion in industrial methylated spirits, lead-free petrol, ethyl acetate, 10% acetic acid, xylene, lubricating oil, paraffin, and water at 23°C, 60°C, and 90°C, together with tropical weathering, heat ageing at 70°C, and testing from -40°C to 100°C.
Test results are specific to the stated exposure media, duration, substrate preparation, cure schedule, and test temperature.
Next steps

Evaluate ARALDITE 2022-1 for your bonding process

Contact Krayden to discuss substrate preparation, bondline design, dispensing equipment, cure timing, and testing for your specific assembly. Product suitability should be confirmed under the actual materials, joint geometry, production conditions, and service environment.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers