ALPHA UP-78 Solder Paste Flux

Harmonization Code : 3810.10.00 | Soldering, brazing or welding powders and pastes consisting of metal and other materials

ALPHA UP-78 Solder Paste

Main features

  • Stable Tack Across Production Shifts
  • Clear, Colorless, Penetrable Post-Reflow Residue
  • Standard and Fine-Pitch Stencil Printing

Product Description

ALPHA® UP-78 No-Clean Solder Paste Flux is a stencil-printing solder paste developed for surface-mount assembly with air reflow and no required post-reflow cleaning. It produces a clear, colorless, soft, and non-tacky residue engineered for penetration during automated test equipment pin testing. The formulation maintains stable tack and printing performance during extended production shifts and is tolerant of varied reflow profiles across different board designs.

Key features

  • Extended printing performance: Provides long stencil life and stable tack with minimal performance change over eight-hour shifts under varying humidity exposure.
  • ATE-compatible residue: Produces a highly penetrable, soft, non-tacky residue designed to reduce false rejects during pin testing.
  • Flexible reflow processing: Tolerates a variety of reflow profiles for use across different surface-mount board designs.

Applications / Suitable for

  • Stencil printing for surface-mount assembly
  • Air-reflow processes where post-reflow cleaning is not required
  • Standard and fine-pitch printing
  • Assemblies requiring automated pin-test compatibility

Technical Specifications

General Properties
Color
The color
pale, off white
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.99
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
380-500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Published properties of ALPHA® UP-78 Paste Flux before reflow.

Property Value Unit Method / condition
Color Pale, off-white — Published chemical property
Specific gravity 0.99 g/cc Published chemical property
Viscosity 380–500 poise 5 RPM at 25°C
Tack strength >6 g/mm² Published technical data
Stencil life Approximately 8 hours 40–60% RH and 20–25°C
Halide content 550 ppm Published technical data
Water content 0.2 maximum % Published technical data
Flux classification REL1 — IPC J-STD-004
Shelf life 6 months Unopened sealed container; avoid temperatures above 27°C (80°F)

 

Technical properties

After-processing / final-state properties

Published residue and electrical test results after reflow without cleaning.

Property Value Unit Method / condition
Reflowed residue Tack-free — After reflow
Corrosivity Pass — Copper mirror test
Surface insulation resistance >2 × 109 Ω IPC J-STD-004; 7 days, uncleaned, comb down
Surface insulation resistance >3 × 109 Ω IPC J-STD-004; 7 days, uncleaned, comb up
Surface insulation resistance >1 × 1012 Ω Bellcore; 4 days, uncleaned, comb down
Surface insulation resistance >3 × 1012 Ω Bellcore; 4 days, uncleaned, comb up
Electromigration Pass — Bellcore; 500 hours