ALPHA LONCO RF-800 FLUX

Harmonization Code : 3810.90.90 | Fluxes and other auxiliary preparations for soldering, brazing, welding

ALPHA LONCO RF-800 FLUX GALLON YELLOW

Main features

  • Highly Active Low-Solids No-Clean Flux
  • Low Non-Tacky Residue
  • IPC J-STD-004 ROL0 Classification

Product Description

ALPHA® ROSIN FLUX 800 (RF-800) is a highly active, low-solids, no-clean liquid flux formulated for wave soldering in tin-lead and lead-free electronics assembly processes. Its proprietary activator system supports soldering across a broad operating window, including assemblies with less-solderable component leads and pads. RF-800 is particularly suited to bare copper boards protected with organic or rosin/resin coatings and tin-lead-coated PCBs. After soldering, it leaves a low level of non-tacky residue that can remain on the assembly and is readily penetrable during pin testing.

Key features

  • Highly active no-clean formulation: Supports effective soldering with less than 5% solids while eliminating the normal requirement for post-solder cleaning.
  • Broad process compatibility: Suitable for tin-lead and lead-free wave soldering with foam, wave, or spray flux application methods.
  • Low, non-tacky residue: Leaves residue designed to remain on the board with reduced interference during pin testing.

Applications / Suitable for

  • Tin-lead and lead-free wave soldering
  • Bare copper PCBs protected with organic or rosin/resin coatings
  • Tin-lead-coated printed circuit boards
  • Foam, wave, and spray fluxing processes

 

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
pale yellow liquid
Solids
4.1 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.794
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
13 °C

Additional Information

 

Technical properties

As-supplied / before-processing properties

Typical properties of ALPHA RF-800 in its as-supplied liquid state.

Property Value Unit Method / condition
Appearance Pale yellow liquid — Typical
Solids content 4.1 % wt/wt Typical
Acid number 18.0 ± 1.0 mg KOH/g Typical
Specific gravity 0.794 ± 0.003 — At 25°C (77°F); typical
pH 3.4 — 5% aqueous solution; typical
Flash point 13 (56) °C (°F) T.C.C.; typical
Shelf life 540 days From date of manufacture

 

Technical properties

After-processing / final-state properties

Corrosion and electrical reliability results obtained with SAC305 alloy and uncleaned test boards under the stated test conditions.

Property Value Unit Method / condition
Silver chromate paper test Pass — No halide detected; SAC305 alloy
Copper mirror test Pass — No complete removal of copper; SAC305 alloy
IPC copper corrosion test No corrosion — Type L result; SAC305 alloy
Surface insulation resistance, comb-down 1.1 × 1010 Ω IPC J-STD-004A; uncleaned; 85°C/85% RH for 7 days; −50 V bias; measured at 100 V on IPC B-24 board
Surface insulation resistance, comb-up 9.8 × 109 Ω IPC J-STD-004A; uncleaned; 85°C/85% RH for 7 days; −50 V bias; measured at 100 V on IPC B-24 board
Bellcore electrochemical migration resistance Pass — TR-NWT-000078, Issue 3; uncleaned; 85°C/85% RH for 500 hours; 10 V bias; measured at 100 V on IPC B-25 B-pattern boards

 