ABLESTIK KS 4008

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK KS 4008

Main features

  • 0.01 ohm-cm Conductive Bonding
  • Aircraft Static-Discharger Bonding
  • Room-Temperature or Heat Cure

Product Description

LOCTITE® ABLESTIK KS 4008 is a two-component, silver-filled epoxy adhesive developed for bonding static dischargers to aircraft. The electrically conductive system combines a cured volume resistivity of 0.01 ohm-cm with aluminum-to-aluminum tensile lap shear strength of 10.3 N/mm² after curing for 2 hours at 60°C. It mixes at 100:6 by weight and provides a 60-minute working time for a 28 g mixed mass at 25°C. Room-temperature and heat-cure schedules are available, with a documented operating-temperature range of -55 to 125°C.

Key features

  • Electrically conductive formulation: Silver-filled epoxy provides a typical cured volume resistivity of 0.01 ohm-cm.
  • Documented bonding performance: Aluminum-to-aluminum tensile lap shear strength reaches 10.3 N/mm² after curing for 2 hours at 60°C.
  • Room-temperature or heat cure: Guideline cure schedules include 24 hours at 25°C or 2 hours at 60°C.

Applications / Suitable for

  • Bonding static dischargers to aircraft
  • Aircraft assemblies requiring protection against electrostatic discharge
  • Electrically conductive adhesive assembly

Technical Specifications

General Properties
Density (g)
2.9 g/cm3
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100 : 6
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
3.65
Work life @25°C
Work life is the amount of time we have to work with a material until it is no longer able to be easily worked and applied on a substrate. It is based on the change in viscosity and it can rely on the application requirements.
1 hours
Thermal Properties
Operating Temperature
-55 to 125 °C
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
0.01 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties and processing characteristics of the individual components and mixed adhesive before cure.

Property Value Unit Method / condition
Appearance — Component A Silver — Resin component, as supplied
Appearance — Component B Amber — Hardener component, as supplied
Filler type Silver — Epoxy adhesive system
Mix ratio — Component A:Component B 100:6 by weight Two-component system
Viscosity — Component B 7,000 mPa·s (cP) Brookfield RVF, ASTM D2393; spindle 5, 4 rpm at 25°C
Working time 60 minutes 28 g mixed mass at 25°C
Shelf life — Component A 365 days At 25°C
Shelf life — Component B 365 days At 25°C
Cure schedule 24 hours or 2 hours — 24 hours at 25°C or 2 hours at 60°C; guideline recommendations
Technical properties

After-processing / final-state properties

Typical cured-material properties and performance results. Values are reference data and are not product specifications.

Property Value Unit Method / condition
Operating-temperature range -55 to 125 °C Documented product range
Volume resistivity 0.01 ohm-cm Cured material; test method not stated
Tensile lap shear strength — aluminum to aluminum 10.3 (1,500) N/mm² (psi) Cured for 2 hours at 60°C
Tensile lap shear strength — aluminum to aluminum 8.3 (1,200) N/mm² (psi) Cured for 24 hours at 25°C