3M EZ250150

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M EZ250150

Main features

  • Extended 2 to 4 Minute Open Time
  • Aluminum or Glass to Wood or Plastic
  • Flexible Cured Adhesive Layer

Product Description

3M Scotch-Weld PUR Easy 250 Plastic Adhesive EZ250150 is a one-component, 100% solids moisture-curing polyurethane reactive adhesive for longer assembly windows on larger or more complex parts. Applied warm at 121 deg C, it provides an open time of 2 to 4 minutes and a set time of 30 to 150 seconds. Supported combinations include wood-to-wood, plastic-to-plastic, wood-to-plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic. A typical elongation at break of 700% after seven days at 23 deg C indicates a flexible cured adhesive layer that can deform before breaking. Moisture access is required, so metal-to-metal, glass-to-glass, and metal-to-glass bonds are excluded.

Key features

  • Longer assembly window: An open time of 2 to 4 minutes and a set time of 30 to 150 seconds support larger or more complex assemblies.
  • Supported substrate combinations: Bonds wood and plastics and joins aluminum or glass to wood or plastic while preserving moisture-access limits.
  • Flexible cured adhesive layer: A typical 700% elongation at break indicates a cured layer that can deform before breaking rather than acting as a rigid bondline.

Applications

Applications include larger or more complex wood, plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic assemblies that benefit from the longer open and set window.

Technical Specifications

General Properties
Color
The color
White / Off - White
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
9,000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
700 %

Additional Information

Technical properties

As-supplied / before-processing properties

Open and handling times are approximate and depend on adhesive temperature and application conditions.

PropertyValueUnitMethod / condition
Color, solidWhite to off-whiteAs supplied
Viscosity9,000cP121 deg C; Brookfield Thermosel, spindle No. 27
Density, molten9.1lb/galTypical
Solids content100%Typical
Application temperature121deg C250 deg F
Open time2 to 4minutesProduct feature range
Set time30 to 150secondsProduct feature range