3M EZ250120

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M EZ250120

Main features

  • Medium-Set Wood Assembly
  • Thin-Bondline Warm Application
  • Moisture-Curing One-Part Processing

Product Description

3M Scotch-Weld PUR Easy 250 Wood Adhesive EZ250120 is a one-component, 100% solids moisture-curing polyurethane reactive adhesive for wood, wood-based surfaces, and selected plastics. Applied warm at 121 deg C, its low-viscosity melt is designed for thin glue lines. The supported open-time range is 1.5 to 4 minutes, and the set-time range is 15 to 120 seconds, providing a medium-set process for wood assembly. Cure rate depends on air temperature, relative humidity, substrate type, and bondline thickness. Moisture must reach the bondline; the adhesive is not suitable for metal-to-metal, glass-to-glass, or metal-to-glass bonding because those substrate pairs do not provide enough moisture for cure.

Key features

  • Medium-set assembly window: An open time of 1.5 to 4 minutes and a set time of 15 to 120 seconds support efficient wood assembly.
  • Thin glue-line processing: A typical viscosity of 3,000 cP at 121 deg C supports controlled application in thin bondlines.
  • Moisture-dependent cure: Cures with available moisture, defining suitable substrate pairs and excluding metal-to-metal, glass-to-glass, and metal-to-glass bonds.

Applications

Applications include wood and wood-based assembly, thin glue-line bonding, and selected plastic bonding where the joint and process provide moisture for cure.

Technical Specifications

General Properties
Color
The color
White/ Off - White
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
3000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
625 %

Additional Information

Technical properties

As-supplied / before-processing properties

Open and handling times are approximate and depend on adhesive temperature and application conditions.

PropertyValueUnitMethod / condition
Color, solidWhite to off-whiteAs supplied
Viscosity3,000cP121 deg C; Brookfield Thermosel, spindle No. 27
Density, molten8.9lb/galTypical
Solids content100%Typical
Application temperature121deg C250 deg F
Open time1.5 to 4minutesProduct feature range
Set time15 to 120secondsProduct feature range