3M EC-5816

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-5816

Main features

  • Flexible Abrasion-Resistant Protection
  • Spray Brush or Flow Application
  • 30-Minute Tack-Free Drying

Product Description

3M Scotch-Weld Elastomeric Coating EC-5816 is a one-part synthetic-elastomer coating for polyurethane foam, glass wool, cork, and other fragile porous insulation materials. It forms a tough, flexible layer that resists abrasion, heat, flame, weathering, water, gasoline, aircraft fuel, and specified lubricating fluids under the stated conditions. The coating can be sprayed, brushed, or flow coated; spray application is recommended for foam. It becomes tack-free in about 30 minutes and should dry for at least 48 hours before service. A typical 3 to 5 mil coating is built in multiple coats with drying between passes. The product can also be applied to primed metal.

Key features

  • Flexible abrasion-resistant protection: Forms a tough, flexible coating that protects fragile porous insulation from abrasion during service.
  • Spray, brush, or flow application: Offers multiple application methods, with spray application recommended for polyurethane foam.
  • Defined drying before service: Reaches a tack-free state in about 30 minutes and requires at least 48 hours of drying before service.

Applications

Applications include protective finishing of polyurethane foam, glass wool, cork, and other porous insulation materials in aerospace manufacturing and maintenance, as well as coating primed metal.

Technical Specifications

General Properties
Color
The color
White
Density (g)
0.97 to 1.04 g/cm3
Solids
26.5-30.5 %
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
50-500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorWhiteAs supplied
Density8.1 to 8.7 (0.97 to 1.04)lb/gal (g/cm^3)Typical
ConsistencyThin liquidAs supplied
Viscosity50 to 500cPBrookfield RVF No. 2 spindle at 20 rpm
Solids content26.5 to 30.5%Typical
Technical properties

After-processing / final-state properties

Values are typical for an approximately 5 mil free film cured for 4 days at 25 +/- 1 deg C, unless another condition is shown.

PropertyValueUnitMethod / condition
Tensile strength2,000 (13.8)psi (MPa)ASTM D638; approximately 5 mil free film, cured 4 days at 25 +/- 1 deg C
Elongation350%ASTM D638; approximately 5 mil free film, cured 4 days at 25 +/- 1 deg C
Tear strength250 (1,112)lb/in (N/25 mm)Approximately 5 mil free film, cured 4 days at 25 +/- 1 deg C
Abrasion index10.0mgCS-17 wheel; 1,000 g load; 100 cycles
Moisture vapor transmission10.0g/m^2/24 hASTM E96-63T, Procedure A