3M EC-1751

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-1751

Main features

  • Metal Repair And Void Filling
  • Controlled Thick Paste Placement
  • Flexible Ambient Or Heat Cure

Product Description

3M Scotch-Weld Epoxy Adhesive EC-1751 B/A is a gray, aluminum-filled two-part epoxy for structural metal bonding, void filling, and repair of holes, dents, and cracks. Mix Part B and Part A at 3:2 by volume or 2:1 by weight; the thick paste remains where applied and provides approximately 45 minutes of work life at 24 deg C. Handling strength develops in 8 to 12 hours. After cure, the adhesive reaches Shore D 75 to 80 hardness and 2000 psi overlap shear on prepared aluminum at 24 deg C.

Key features

  • Metal Repair And Void Filling: The aluminum-filled paste supports holes, dents, cracks, and irregular bondlines.
  • Controlled Thick Paste: High viscosity helps keep the adhesive in place during assembly.
  • Room Temperature Or Heat Cure: The two-part epoxy supports ambient cure or faster controlled heat schedules.

Applications

Structural bonding of prepared metals, composites, and selected plastics; metal-hole repair; dent filling; and crack repair.

Technical Specifications

General Properties
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two (Amine / Epoxy)
Other Properties
Storage Temperature
16 - 27 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Part B colorGray-Before mixing
Part A colorAmber-Before mixing
Mix ratio by weight2:1B:ATwo-part system
Mix ratio by volume3:2B:ATwo-part system
Part B density10.8lb/galAs supplied
Part A density7.9lb/galAs supplied
Work lifeApproximately 45minAt 24 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
Hardness75 to 80Shore DCured
Thermal conductivity0.2229BTU/hr/ft2/deg F/ftAt 36 deg C
Overlap shear strength2000psiAluminum; ASTM D1002; tested at 24 deg C
T-peel strength4piwAluminum; ASTM D1876; tested at 24 deg C
Time to handling strength8 to 12hAt room temperature

Leading Brands Trust in Our Products and Services