3M AF325LS.59

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M AF325LS.59

Main features

  • Integrated Composite Surfacing Layer
  • Smooth Low Porosity Finish
  • Configuration Specific Lightning Protection

Product Description

3M Scotch-Weld Composite Surfacing Film AF 325LS, 0.059 wt is a thermosetting epoxy surfacing film for composite aircraft structures. The preformed layer supports a smooth, low-porosity surface that can reduce finishing work before painting. AF 325LS constructions may incorporate a conductor for lightning-strike protection when the complete LS configuration is specified. The 0.059 wt designation identifies the intended commercial construction, while the conductor, color, liner, and complete part code remain essential selection details for layup and cure planning during aerospace composite manufacturing.

Key features

  • Integrated Composite Surfacing Layer: The preformed thermoset film creates a controlled exterior layer during composite cure.
  • Smooth Low Porosity Finish: The cured surface supports reduced preparation before painting.
  • Configuration Specific Lightning Protection: LS constructions can integrate a conductor when the complete configuration is specified.

Applications

Composite aircraft surfacing and lightning-strike protection with the exact conductor-equipped LS construction.

Product Family

3M AF325LS.59

Loading pricing…

Technical Specifications

Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
152 °C
General Properties
Film Thickness
Film thickness is the thickness of a backing film without taking into account any coatings or adhesive layers. It is measured in micron and the conversion factor to mil is 0.039.
0.15-0.20 mm

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers